Cube2--C17200 (CDA 172) Beryllium Copper is the most commonly utilized Copper Beryllium alloy and is notable for its highest strength and hardness compared to commercial copper alloys. C17200 alloy contains appr. 2% of beryllium and achieves its ultimate tensile strength can exceed 200 ksi, while the hardness approaches Rockwell C45. Meanwhile, the electrical conductivity is a minimum of 22% IACS in the fully aged condition.C17200 also exhibits exceptional resistance to stress relaxation at elevated temperatures.
International Specification:
Rods/Bars/Tubes: ASTM B196,251,463; SAE J461,463; AMS 4533,4534,4535; AMS4650,4651;
RWMA Class 4
Strips:ASTM B194, AMS4530,4532; SAE J461,463
Sheets: ASTM B194
Wires:ASTM B197, AMS4725, SAE J461,463
Plates:ASTM B194, SAE J461,463; AMS4530,4533,4534,AMS4650,4651; RWMA Class 4.
European Standards: CuBe2, DIN 2.1247, CW101C to EN
Note:
ASTM: American Society for Testing and Materials
SAE: Society of Automotive Engineers
AMS: Aerospace Materials Specification (Published by SAE)
RWMA: Resistance Welder Manufacturers' Association
Note: Unless otherwise specified, material will be produced to ASTM.
Available Sizes:
Custom Diameter & Sizes, Random Mill lengths
Available Products (forms):
Round bars, Round strips, Round wires, Round tube,
Flat bars, Square bars, Rectangular bars, Hexagon bars, Plates, Sheets, Coils
Custom shapes are available upon request.
Chemical Composition:
Be: 1.85-2.10%
Co+Ni: 0.20% Min.
Co+Ni+Fe: 0.60% Max.
Cu: Balance
Note: Copper plus additions equal 99.5% minimum
Typical Physical Properties:
Density (g/cm3): 8.36
Density before age hardening (g/cm3): 8.25
Elastic Modulus (kg/mm2 (103)): 13.40
Thermal Expansion Coefficient (20 ípC to 200 ípC m/m/ípC): 17 x 10-6
Thermal Conductivity (cal/(cm-s-ípC)): 0.25
Melting Range (ípC): 870-980
Note:
1). the units are based upon Metric.
2). the typical physical properties apply to age hardened products.
CuCo1Ni1Be--CW103C (DIN 2.1285) Cobalt Nickel Beryllium Copper Alloy contains approximately 1% Cobalt, 1% Nickel and 0.5% Beryllium. After hot forging and heat treatment processes this material gains considerably hardness, electrical and thermal conductivity as well. It is possible to have different combinations of electrical conductivity and hardness by changing the heat treatment conditions;CuCo1Ni1Be also Offers good strength and hardness characteristics coupled with conductivity in the range of 45-60 percent of copper with ultimate tensile and hardness properties approaching 140 ksi and RB 100 respectively, all of its properties are quite the same as CuCo2Be-C17500 and CuNi2Be-C17510.
International Specification:
Rods/Bars/Tubes: ASTM B441, SAE J461,463; RWMA Class 3
Sheets: ASTM B534
Wires: ASTM B441
Plates: ASTM B534, SAE J461,463; RWMA Class 3
European Standards: CuCo1Ni1Be, DIN 2.1285; CW103C to EN
Note:
ASTM: American Society for Testing and Materials
SAE: Society of Automotive Engineers
AMS: Aerospace Materials Specification (Published by SAE)
RWMA: Resistance Welder Manufacturers' Association
Note: Unless otherwise specified, material will be produced to ASTM.
CuCrNi2Si ¿C UNS.C18000 Copper Chromium Nickel Silicon Alloys, which also called Beryllium Free Copper alloy, meets the mechanical requirements of RWMA Class 3 Copper, is a very hard heat treatable copper based alloy with an economical higher strength and high conductivity, and C18000 Alloys is utilized when a combination of very good mechanical strength along with moderate electrical and thermal electrical conductivity are required. Furthermore, C18000 alloy is an excellent substitute for copper beryllium alloys C17500 and C17510 in terms of many applications.
International Specification:
Rods/Bars/Plates/Sheets: UNS.C18000, CDA180, RWMA Class 3
European Standards: CuCrNi2Si, DIN 2.0855, CW111C to EN
Note:
ASTM: American Society for Testing and Materials
RWMA: Resistance Welder Manufacturers' Association
Note: Unless otherwise specified, material will be produced to DIN & RWMA.
345 Metal Products Suppliers
Short on time? Let Metal Products sellers contact you.
Cube2--c17200 (cda 172) beryllium copper is the most commonly utilized copper beryllium alloy and is notable for its highest strength and hardness compared to commercial copper alloys. C17200 alloy contains appr. 2% of beryllium and achieves its ultimate tensile strength can exceed 200 ksi, while the hardness approaches rockwell c45. Meanwhile, the electrical conductivity is a minimum of 22% iacs in the fully aged condition.C17200 also exhibits exceptional resistance to stress relaxation at elevated temperatures.
Available sizes:
Custom diameter & sizes, random mill lengths
International specification: ú¿¦·+O¦µ+¦ú¬
Rods/bars/tubes: astm b196, 251, 463; sae j461, 463; ams 4533, 4534, 4535; ams4650, 4651;
Rwma class 4
Strips:astm b194, ams4530, 4532; sae j461, 463
Sheets: astm b194
Wires:astm b197, ams4725, sae j461, 463
Plates:astm b194, sae j461, 463; ams4530, 4533, 4534, ams4650, 4651; rwma class 4.
European standards: cube2, din 2.1247, cw101c to en
Note:
Astm: american society for testing and materials
Sae: society of automotive engineers
Ams: aerospace materials specification (published by sae)
Rwma: resistance welder manufacturers' association
Note: unless otherwise specified, material will be produced to astm.
Usage: used in electro, metallurgy and chemical industry.
1. Widely applied to refractory material and power metallurgy industry to improve the heat resistance, wear resistance and oxidation resistance. Products made of it are applied in steel smelting furnace, kiln hood and kiln furniture etc.
2. In the chemical line of organic silicon, industrial silicon powder is basic raw material that high polymer of organic silicon formatting. Such as using for producing organic monomer, silicon oil, silicon rubber antiseptic to improve the characteristics of insulating, corrosion-resistance and waterproof performance etc.
3. Industrial silicon powder is sublimated into monocrystaline silicon, which is widely used in hi-tech field as an essential raw material for integrated circuit and electronic element.
4. In metallurgy and foundry line, industrial silicon powder is regarded as to be iron base alloy additive, the alloy pharmaceutical of silicon steel, thus improve the steel hardenability
(1)no mark or mark as client's requirement
(2)1mt/bag or as client's requirement
(3)plastics woven bag
CuSn5 UNS.C51000 Phosphor Bronze Alloys, with a nominal composition of 94.80% copper and 5.0% tin, deoxidized with 0.2% phosphorus is the most widely used of the phosphor bronzes, which offering an optimum combinations of such engineering properties as high strength and ductility.
CuCr1Zr UNS.C18150 Chromium Zirconium Copper C18150 is an excellent and unique copper alloy with high electrical conductivity, hardness, and ductility, moderate strength, and excellent resistance to softening at elevated temperatures. The addition of 0.1% zirconium (Zr) and 1.0% chromium (Cr) to copper results in a heat treatable alloy which may be solution treated and subsequently aged to produce these desirable properties. Rod is usually supplied from the mill in the fully aged and drawn condition so no further heat treatment is required by the fabricator. The softening temperature of properly heat treated C18150 rod exceeds 500ípC as compared to unalloyed pure copper which softens at 200ípC, and silver bearing coppers which soften at 350ípC.
The specs for mg metal ingot shows as below:
Size: 7.5kg+/- 0.5kg/Ingot
Mg : 99.9% Min
Si : 0.02% Max
Al : 0.02% Max
Mn : 0.03% Max
Fe : 0.04% Max
Cl : 0.005% Max
Others each 0.01% Max.
about 1mt in a magnesium pallet, covered with plastic bag, bundle with steel tape.
Grade P1020, A7, A8, A85, ADC12
Origin Malaysia, Australia, South Africa, India, Russia, Middle East
Brand Press Metal/Tomago/Portland/Boyne/Hindalco/Vedanta/Rusal/Alba/Maaden/Sohar/Hillside