Levels
T22/P22
T5/P5
T9/P9
T91/P91
T23/P23T92/P92
Features
Most commonly used , low alloy heat resistant with strong characteristic. Commonly used as heating surface pipes in fire/nuclear /petrochemicals industryGood performance in antioxidant, inoxidability, structure stability as well as perfect processing propertyIts Chrome Content is increased and with better performance in antioxidant, inoxidability than T5, but with weaker heat resistance and welding performance, high anti Coxidantant and anti high temperature corrosion. Stable Toughness / durable plastic / thermal force; T 610,its admissable stress is higher than the austenitic steel, T í¦ 550. Recommended allowable stress of steel is twice as high as that of T9 twice.
In addition to high anti-oxidation, good corrosion resistance, high impact toughness and stable / durable plastic / heat intensity, smelting deformation of micro-alloying to obtain high-density dislocation / highly refined grains, welding performance improved.
Significantly.The increase of W element is significantly improved resistance to high temperature oxidation and to hot corrosion compared with T91. Mo's appropriate decrease improve the stability and availability of welded steel / welded joint. B is the strong element temperature which highly improve the resistance to elevated temperature creep. Its resistance to lasting / creep / corrosion resistance is better than T91.
We can offer 21"-48".
Used in structure or chemical aspects.
We can offer 1/2"-24".