NICKEl - IRON ALLOY KOVAR Composition (Nominal): NI 29; Co17; Fe Balance;) ;(A low expansion alloy which has been widely used for making hermetic seals with the harder Pyrex glass and ceramic materials such as in power tubes, microwave tubes, transistors, and diodes, as well as integrated circuits. :) (Specifications: Kovar alloy is manufactured to meet the requirements of ASTM Specification F-15.
SOFT MAGNETIC - IRON COBALT ALLOY Permendur 49 : (Composition (Nominal): Fe49; V2; Co49:) :(PERMENDUR 49 exhibit the highest magnetic saturation (2.4 T) of all soft-magnetic alloys. high D.C. maximum permeability, low D.C. coercive force, and low A.C. core loss. : (Specifications: ASTM A801 Alloy Type 1 ; ( Please request a QUOTE for material Datasheet ?
ron Nickel alloy ASTM F30 alloy 46 ;( Composition (Nominal) Ni 46 ; Fe Balance: ( Alloy 46 is a nickel-iron controlled expansion alloy containing 46% nickel. It has a fairly constant coefficient of thermal expansion from room temperature up to 500 °C. ; : (SPECIFICATION: ASTM F30
Glass Sealing 42 Alloy :(Composition (Nominal): 0.05 C, 0.40 Mn, 0.25 Si, 41.0 Ni, Bal. Fe; : ( Alloy 42 A nickel-iron controlled-expansion alloy containing 41% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 300°C.Used for glass-to-metal sealing of components that are enclosed in a glass envelope,such as lamps and electron tubes. :(Specification : ASTM F30 ; ( Product availability and request a QUOTE!
Nilo 42 Alloy :(Composition (Nominal): 0.05 C, 0.40 Mn, 0.25 Si, 41.0 Ni, Bal. Fe; : ( Nilo 42 A nickel-iron controlled-expansion alloy containing 41% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 300°C.Used for glass-to-metal sealing of components that are enclosed in a glass envelope,such as lamps and electron tubes. :(Specification : ASTM F30 ; ( Product availability and request a QUOTE!
INVAR 42 Alloy :(Composition (Nominal): 0.05 C, 0.40 Mn, 0.25 Si, 41.0 Ni, Bal. Fe; : ( INVAR 42 A nickel-iron controlled-expansion alloy containing 41% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 300°C.Used for glass-to-metal sealing of components that are enclosed in a glass envelope,such as lamps and electron tubes. :(Specification : ASTM F30 ; ( Product availability and request a QUOTE!
Nickel Iron Alloy 48 UNS K94800/ Nilo 48 ASTM F30 ; ( Composition (Nominal): Ni48 ; Fe Balance ; )Alloy 48 (Nilo 48) is a low expansion Nickel-Iron alloy. The coefficient of thermal expansion of this metal is designed to suit the CTE of soft lead and soda lime glasses. High Inflection point. Its service temperature goes as high as up to 450oC or 840oF. : (Product availability and request a QUOTE!
SOFT MAGNETIC IRON COBALT ALLOY Hiperco 50A ; (Composition (Nominal): Fe49, V2 , Co 49, :)Hiperco 50A Alloy is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (2.4T), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core loss. :) Specifications: ASTM A801 Alloy Type 1 ;( Product availability and request a QUOTE!
NICKEL IRON SEALING ALLOY 52 ; (Composition (Nominal): Ni 50 , Fe Balance . ;( Alloy 52 is a 50% nickel-iron alloy developed for glass-to-metal seals for some of the soft glasses and some ceramics. The alloy's rate of thermal expansion is virtually constant to a temperature of about 1050 °F (565 °C). ;(Specification : ASTM F30 ; ;(Product availability and request a QUOTE!
IRON NICKEL ALLOY ASTM F1684 INVAR 36 ; (Composition (Nominal): 0.02 C, 0.35 Mn, 0.20 Si, 36.00 Ni, Bal. Fe ; ( Invar (also know as Invar 36, NILO 36, Pernifer 36, and Invar Steel) is a low expansion alloy consisting of 36% Nickel, balance Iron. Invar Alloy exhibits extremely low expansion around ambient temperatures, making Invar Alloy particularly useful in applications where minimum thermal expansion and high dimensional stability is required, such as in precision instruments like optoelectronic devices, optical and laser benches, electronics, and other kinds of scientific instruments.; ( SPECIFICATION: astm f 1684 ; (Product availability and request a QUOTE!
IRON NICKEL ALLOY ASTM F1684 PERNIFER 36 ; (Composition (Nominal): 0.02 C, 0.35 Mn, 0.20 Si, 36.00 Ni, Bal. Fe ; ( Invar (also know as Invar 36, NILO 36, Pernifer 36, and Invar Steel) is a low expansion alloy consisting of 36% Nickel, balance Iron. Invar Alloy exhibits extremely low expansion around ambient temperatures, making Invar Alloy particularly useful in applications where minimum thermal expansion and high dimensional stability is required, such as in precision instruments like optoelectronic devices, optical and laser benches, electronics, and other kinds of scientific instruments.; ( SPECIFICATION: astm f 1684 ; (Product availability and request a QUOTE!
Iron-Nickel-Chromium alloy NI SPAN C902 UNS N09902 .,;( Composition (Nominal): Ni 43 ., Cr 6., Ti 3. Fe Balance ., :( Ni-Span C902 nickel iron chromium alloy is precipitation hardenable. It can attain controlled thermoelastic coefficient and static elastic modulus at temperatures from -50° F to 150° F. The main constituents of alloy are iron, nickel and chromium with nominal traces of titanium and aluminum. These elements produce a reddish-brown oxide layer upon exposure to natural conditions since it does not have the same qualities as stainless steel. Additionally, nickel iron chromium alloys feature nominal expansion after hot and cold processing. (Product availability and request a QUOTE!
Metal alloys.
Ferromolybdenum .Commodity market trading
Ferro alloy.
Heeralloys.
Potassium bifluoride / all kind of rare earth/ ferro alloy.
Metal alloys.
Ferroalloy (fesi, fecr, femn, si metal, mn metal, si ca,si ba,cr metal , simn).Cif, fob
Ferro alloys.