Antioxidant d Molecular formula : c16h13n Chemical name: n-phenye---naphthylamine Executive standard: q/12hg 4521-2001 Specification: Index grade Appearance gray to red powder Initial melting point ¦ 105.0 Loss on heating % 0.20 Ash content % 0.20 Residue on sieve(100m) % 0.20 Application: it is widely used in all kinds of natural rubber and synthetic rubber. It has good preventing performance caused by heat, oxidizing and wind. It also can be used for making some black rubber products. Package and storage: 25kg paper bag in lined with plastic bag. It should be stored in a cool, well-ventilated area.
Antioxidant sp Molecular formula: c30h30o Chemical name: styrenated phenols Executive standard: q/hg 16-254-82 Specification: Index grade First second Appearance pale yellow clear heavy-solid Viscosity (pt) 30-50 20-39;51-60 Refractive indexd2 1.5985-1.6020 Specific weigh 1.07-1.09 Ash content %_ 0.50 1.00 Application: it is a stabilizer of synthetic rubber includin sbr neoprene and ethylene-propylene rubber and natural rubber. It+s very good ageing resistance properties for rubber products and emulsion products. Can improve product+s heat proof, oxidation resistance and ageing resistance performance, it has the advantage of noncoloring, nonpolluting and easy dispersion, it can be used in emulsion after emulsification. Package and storage:25kg paper bag in lined with plastic bag. It should be stored in a cool well-ventilated area.
Accelerator m(mbt) Accelerator m(mbt) Molecular formula c7h5ns2 Chemical name 2-mercaptobenzothiazole Executive standard gb/t 11407-2003 Specification Index grade Appearance pale yellow or white powder or crystal First conformity Inital m.P(¦)171.0 170.0 Ash content% _ 0.30 0.30 Loss on heating _ 0.40 0.50 Residue on sieve(150m)% _ 0.10 0.10 Application: being a general type of accelerator. This product has rapid promoting function for natural rubber and common valcanized rubber. It should be stored in the place of cool, dry& good ventilated and away from fire. We also are supplying granular and oily products. Net weight:20kg. Package and storage: the outer is a woven bag, the inner is a plastic bag.
Rubber additive 25KG Per Bag
Epdm colorful rubber granule Acetone extract: 10% Ash content: 65% Polymer content: chlorination butyl and epdm Tensile strength: 30mpa Glue content: 15% Elongation at break: 150% Hardness: 55f¼70a Sizes: 0.5-1.5mm 0.5-2.5mm 1-3mm 2-4mm 3-5mm Colors: Red green blue yellow gray etc Country of origin: china Packaging: We packed 25 kg per piece in p.P bag. One 20ft container can fill with 20 tons of our products. Volume: Each pallet is 1.6cbm of lcl
Supplying rubber chemicals with high quality and competitive price 25kg/bag
Rubber antioxidant 4010na (ippd) Chemical namen-isopropyl-n¹-phenyl-p-phenylene-diamine Molecular formulac15h18n2 Synonyms: ippd Molecular weight 226.4 Cas no: 101724 ; Einecs no. 2029697 Standardgb8828--88: Specification: Assay value: 95%min Appearance: purple-brown granule Melting point: 70f¦ min Heating loss: 0.5% max Ash content: 0.3% max Packed in kraft paper 25kg per bag lined with pp woven bag with plastic bag inside and storage in cool and dry conditions.
Rubber antioxidant tmq/rd Rubber antioxidant rd (polymerized-2, 2, 4-trimethyl-1, 2-dihydroquinoline resin) 1f=molecular formula(c12h15n)n. N=2f+4. 2f=specilication:(gb8826-88) Item high grade ist grade Appearance amber to brown flake Soften point 80f+100 80f+100 Reduction in weight after heating, %f_ 0.30 0.50 Ash, %f_ 0.30 0.50 3properties:amber to brown flake or powder. Gravity 1.05, solube in benzol, chloroform and acetone, nonsoluble in water, but little soluble in petrolem hydrocarbon. 4 application:the product is mainly used for natural rubber, butadiene nitrile and chloroprene rubber etal, used in tyres, industry rubber and so on. pacdage: polypropyrene knitted bags lined with polyethylene bags. Net weight 25kg per bag
Rubber antioxidant d Rubber antioxidant d (n-phenyl-2-naphthylamine) 1f=molecular formula:c16h13n 2f=specification:(hg2-469-79) Item specification Appearance pale or brown powder Melting point, 0f¦fª 105.0 Reduction in weight after heating, %f_ 0.20 Ash, %f_ 0.20 Phenylamine content no blue and purple reaction by testing Screen residue(100 meshes), %f_ 0.2 Magnetic object content, %f_ 0.008 3f=properties:pale powder, boiling point 365.5f¦. Soluble in acetone, chloroform, alcohol and tetracol, nonsoluble in gasoline and water. 4f=application:the product is mainly used for natural and synthetic. Used in tyres, rubber belts, rubber shoes and so on. Package:polypropyrene knitted bags lined with polyethylene bags. Net weight 25kg per bag.
Rubber chemicals
Characterwhite or pale yellow crystals, soluble in acetone, benzene, toluene, ether and ethyl acetate, and warm carbon tetrachloride, ethanol and heptane. It is slightly soluble in gasoline and insoluble in kerosene and water. Applicationthis product can be used in natural rubber and synthetic rubber. It can effectively prevent the burning of rubber compound in the process of processing, thus making it possible for calender and extruder to operate at high temperature and high speed, improving the production capacity of vulcanizer, improving the storage stability of rubber compound, preventing natural vulcanization during storage, and for rubber which has already undergone high heat or has the risk of scorching.The material has regeneration effect.
Molecular Formula: C5H8 The goods is an important monomer of synthetic rubber, its dosage accounted for 95% of the total output of isoprene, mainly used for the synthesis of isoamyl rubber, its production after styrene-butadiene rubber and butadiene rubber and synthetic rubber in the third.Secondly, used as a monomer synthesis of butyl rubber, to improve the butyl rubber vulcanization performance, but very few dosage, isoprene is also used in synthetic resin, liquid polyisoprene rubber, etc.Also used in the manufacture of pesticide, medicine, spices, adhesives, etc.
Silane coupling agent Silane coupling agent Si-69 chemistry is named double [gamma - (triethoxy silyl) propyl] four sulfide.It is often used to treat inorganic fillers such as carbon black and SiO 2. It not only has the function of activator and coupling agent, but also has the function of crosslinking agent, softener and reinforcing agent. It is used as reinforcing agent and vulcanizing agent in rubber industry.
Recommended usage: RH100 is beneficial to improve the mixing uniformity of rubber compounds with different polarities and different viscosities. Through the surface wetting can be quickly absorbed by the rubber compound, speeding up the rapid combination of ingredients in the rubber compound formulation. RH100 reduces the Mooney viscosity of the material, improves the fluidity of the rubber compound, and makes the process of calendering and extrusion after mixing easier. It is recommended that RH100 be added at the beginning of the mixing cycle to achieve the best wetting effect.
Application: This product is a general amine antioxidant with excellent heat, oxygen and aging properties in rubber industry. It is especially suitable for all-steel and semi-steel radial tires, and is widely used in tires, hoses, belts, rubber shoes, rubber products and other general industrial rubber products, as well as latex products.
Qualification description: Glue T-78E is a dispersing additive with double dispersing effect on carbon black and inorganic filler. It not only has internal and external lubrication, but also has chemical bonding of functional polymers. It is an economical high-efficiency dispersion. Additives to improve the dispersibility of the powder in the compound, especially the dispersion of carbon black. Glue T-78E can effectively shorten the mixing time, increase the rolling and pressing speed, reduce the extrusion temperature, improve the utilization factor of equipment, reduce energy consumption and cost.
Function: Zno-80, as a natural and synthetic rubber active agent, can improve the crosslinking density and strength of vulcanized rubber. Application: can be used in most rubber products. Storage: store for at least one year under cool and dry condition.
Packaging and storage: paper plastic composite bags, pearlescent film or plastic woven bags, 25kg/ bags. Store in dry and ventilated places. For other types of vulcanization accelerators such as MBT (M), MBTS (TM), DCBS (BZ), TBBS (NS), etc., please send message to Email.
Usage and dosage 1. L-810 is added together with small materials such as zinc oxide when mixing the masterbatch. 2.L-810 is used for tire crown and side rubber, adding 2 ~ 3 parts according to 100 parts of raw rubber;L-810 has no effect on the physical and mechanical properties and vulcanization properties of rubber products. 3. Apply reference tire usage on the conveyor belt.
Product performance: This kind of product can promote the mixing of different polar rubber, improve its compatibility and process performance. It is suitable for mixing, smelting and calendering operations. It can make the binder bond more closely, so as to improve the effect of mixed coal layer seam, disperse better, mix more evenly, and improve the uniformity of the binder. In addition to increasing adhesive viscosity, it can also improve its fluidity and improve the mechanical properties of vulcanized products. In the formulation of butyl rubber, besides improving the processing performance and promoting the dispersion of fillers, it can keep low modulus and maintain good viscosity after aging, improve the extrusion performance, flexibility resistance and air tightness of the rubber. In addition, it can improve the forming viscosity of synthetic rubber, and has excellent dispersing effect on carbon black and mineral filler, without affecting the low-temperature buckling property.