Commodity -iron ore grade fe 57% rejection below fe 56% Origin - goa Description- 57% fe grade iron ore rejection below 56% fe Chemical composition (on dry basis) A. Fe 57% rejection below 56%fe B. S1o2- 7% max C. A12o3- 4% max D. P:0.07% E. S:0.07% F. Moisture - 9% Physical composition (size) - 10 mm : 100% max + 10 mm : 35% min - 0.15 mm : 35% max Fines between 0-10 mm 2 shipment of 55000 mt available. Contact for more details.