Co-based amorphous core in plastic container 1. high permeability 2.Thickness (1820 mkm) 3. Annealing in transverse field, permeability more than 100000, very low loss, flat hysteresis loop 4. Common-mode filter chokes, current transformers, including for precise electronic electricity meters, protective cutout, High Frequency power transformers in SMPS, audio transformers, etc. 5.D from 4-32mm Ribbon wound magnetic core is placed into hard protective container of glass-polyamide and mechanically fixed with silicone sealant. Co-based amorphous ribbon wound magnetic core is placed into hard protective container of glass-polyamide and mechanically fixed with silicone sealant.Size veries:outer D =4-32mm.The container has rounded edges and is designed for direct winding of a thick wire. The container provides reliable mechanical protection and preservation of amorphous material's properties. All materials comply with UL94V-1 / 0. 1. High permeability 2.Thickness (1820 mkm) 3. Annealing in transverse field, permeability more than 100000, very low loss, flat hysteresis loop 4. KEY FEATURES OF THE AMORPHOUS MATERIAL: Induction amplitude, Bm (25C) 0.59 T Induction amplitude, Bm (90C) 0.50 T Curie temperature, Tc 220C Operating temperature range -60C ... 100C Magnetostriction less than 0.110^-6 Typical permeability (10 kHz) - 120 000 Typical permeability (100 kHz) - 35 000