By barium sulfide solution and to join after remove calcium and magnesium mirabilite solution mixing, reaction at 80 â??, precipitate, after the suction filter, washing and acid pickling, adjust pH value 5 ~ 6, filtration, drying and crushing.It can be prepared with barium yellow halogen and glauber solution.