C si mn cr mo v p s
0.45-0.55 0.20-1.00 0.20-0.90 3.00-3.50 1.30-1.80 max 0.35 max0.030 max0.030
Mechanical property
Annealing temperature: 815â°c-845 â°c
Hardness after annealing hbw: 187-233
Quenching temperature: 925â°c-955 â°c
Cooling medium: oil/ air cooling
Tempering temperature: 205â°c-620 â°c
Hardness after tempering hrc: 57-45