1.Commodity: Portland Cement Clinker 2.Specification: - SiO2 (Silicon dioxide): 21.2% - AL2O3 (Aluminum oxide): 5.48 - F2O3 ( Ferric oxide): 3.37% - CaO (calcium oxide): 65.84% - MgO (Magnesium oxie): 1.54% - SO3 ( Sulfur oxide): 0.28% - MKN ( Loss on ignition): 0.47% - CKT (Insoluble residue): 0.13% - CaOtd ( Free limre): 1.36% - C2S: 17.0002 % - C3S: 58.3102% - C3A: 9.0239% - C4AF: 9.7617 % Compresssive strength - after 03 day (± 45 minute) : 36.05 N/mm¬¬2 - after 28 day ( ± 8 Hours) : 55.99 N/mm2 3. Quantity: 25,000 mt ( +/- 5% at sellers option ) 4. Packing: In Bulk