Used in granite and marble anquite effect.
Frankfurt brush adopts dupont filaments; The grain is 36#, 46#, 60#, 80#, 120#, 180#, 240#, 320#, 500# Frankfurt is used in hand and automatic grinding machine
Fickert adopt dupont filaments for antique stone The grain is steel , 36#, 46#, 60#, 80#, 120#, 180#, 240#, 320#, 500#
Characteristics: Granite without machinery¡¢flamed and other pre-treatment processes, using the high abrasive performance of synthetic diamond to grinding the stone surface directly. Application: Processing granite surface into ¡ípleather surface¡í+ effect; The polished granite with more defects; The stone can not be flamed; The stone with a high breakage rate in flamed technology; The stone will discoloration after flamed and so on. Fickert 14cm¡ª¡ªUsed in granite automatic grinding line. Frankfurt¡ª¡ªUsed in hand and automatic grinding machine. Diam.100mm for flex¡ª¡ªUsed in hand grinding machine. Diam.110mm for flex(M14)+snail lock(right)¡ª¡ªUsed in side grinding machine and step retreading machine
Shape: Spherical Color: White / Color-Less Bulk Density: 1.5 -1.6g/cm3 Hardness: 5.5 - 6.0 Moh Finishing: Smoothing Melting Point: 600�°C Material: Clear glass Pattern: Solid Plain Packaging Size: 25 Kg / 50 Kg / 1 Ton Packaging Type: HDPE Woven Gunny Bags Transport Type: Land / Sea / Air Transport Application Surface finishing- Glass Bead blasting can be used on an extended range of substances with glass, plastic, metal, and rubber. The littler the glass spheres, the evener the surface; greater spheres produce an extra textured finish. To defend special areas or in detail aquatint resolves, areas can be effortlessly masked with tape. Cleaning- Glass Bead blasting eliminates foreign elements from the external without a dimensional alteration to the surface. A wide range of bead sizes is available. For example: removing paint, degreasing, light corrosion, and nearly any other surface pollutants. Glass beads may also be utilized to make surfaces for paint adhesion, gasket sealing, or lubrication retention. Deburring- Glass Bead blasting removes burrs, and feathered edges, and alternates from portions in an accuracy process. Corners and edges must be deburred with accuracy to assemble and operate correctly. Glass bead blasting promises that no base metal from the exterior is removed. Gentle and finished areas may be easily masked for protection. Shot peening- Peening with this type of abrasive is a less-cost form of generating an unchanging surface coating of crushed stress in alloy materials. Peening turns to combat stress cracks and rust, resulting in a growing life of metal portions. The high degree of chubbiness of our Glass Bead media progresses the performance of stress confrontation processes.