SiO2 99.46 Fe2O3 0.035 Al2O3 0.233 TiO2 0.052 LOI 0.16 MESH SIZE % Typical Average Retained 40 0.02 50 0.54 60 4.29 70 17.55 80 31.32 100 28.18 140 16.67 200 1.20 PAN 0.23 This silica sand is currently sold to float glass manufacturers and clear bottle manufacturers in the western United States. U.S. Mine Corp is approximately 100 miles from the Port of Oakland and 40 miles from the Port of Stockton.
SiO2 99.51 Fe2O3 0.062 Al2O3 0.324 TiO2 0.072 LOI 0.185 MESH SIZE % Typical Average Retained 40 0.02 50 0.054 60 4.29 70 17.55 80 31.32 100 28.18 140 16.67 200 1.20 PAN 0.72
U.S. Mine Corporation's Ione Airfloated Kaolin Clay is a western U.S based deposit (California) suitable for calcining as a metakaolin and used in high-strength cements. It is available in 50 lb bags, Supersacks, and bulk. SiO2 47.0% Al203 36.31% Fe203 0.55% Ti02 2.4% Ca0 0.05% Mg0 0.03% Alkalies (Na20, K20) 70 Moisture Content (dry) %
Ione Industrial kaolin Clay is a high purity kaolin clay, which is low in iron and alkali content, a run-of-mine kaolin that is sold out of stockpiles. The low iron, low alkali and high aluminum content makes this an ideal kaolin for cement production, and for application in the rubber, fiberglass and agriculture industries. Si02 47.0% Al203 36.31% Fe203 0.55% Ti02 2.4% Ca0 0.05% Na20, K20 70 +325 mesh 5-15% pH (40% solids) 4.0 Moisture Dry 12-16% Raw clay color - white High purity kaolin clay sold in bulk/supersack.
Laterite is an iron-rich mineral used in cement applications and even infield mixes. MgO 0.09 Al2O3 25.64 SiO2 39.73 P2O5 0.13 SO3 0.02 Cl 0.02 K2O 0.15 CaO 0.07 TiO2 1.21 Cr2O3 0 MnO 0.09 Fe2O3 19.52 ZrO2 0.04 LOI 13.30
Lignite is a low-BTU coal used in agricultural applications for its fulvic and humic acid.
USMC has heavy metal sands high in ilmenite available as a raw sand for further processing.
We are glad to propose 500 MT of stain less steel mill scale. Mill scale is formed on the outer surfaces during by the hot rolling lamination of stainless-steel products. At a visual inspection the material is a hard brittle sand and is mainly composed of iron oxides, mostly ferric, and is bluish black in colour, but it also contains considerable alloying elements such as chromium and nickel. The recovery ratio after melting in furnace for the most valuable alloy elements is: - Ni: 3.5 - 4.5% - Cr: 6-8% From the chemical and physical analysis performed on the scrap, and according to the European environmental rules, the material has been classified as a special non dangerous waste, listed in green list. In particular the mill scale can be classified as follows: Waste code: 10 02 10 The material is stored on cemented flooring, and it can be loaded loose in tipper trucks or containers. Chemical analysis of the material is available on request.
Mill scale, is formed on the outer surfaces of plates, sheets or profiles when they are being produced by rolling hot iron or steel billets in rolling or steel mills. It looks like a hard brittle sand and is mainly composed of iron oxides, mostly ferric, and is bluish black in color. Being produced during the reheating, conditioning and hot rolling operation for the production of steel articles, the mill scale initially adheres to the steel surface and protects it from atmospheric corrosion, provided no break occurs in this coating. From the chemical and physical analysis performed on the scrap, and according to the european environmental rules, the material has been classified as a special non dangerous waste, listed in green list In particular the mill scale can be classified as follows: Einecs (european commission no.): 266-007-8 Waste code: 10 02 10 Basel code: b 12 30 Hs code: 2619.00