Raw melting material - aluminum scraps, cans, engine waste etc. Output capacity - 5-30 tons/h, customized Automation - Full automatic/ half automatic (based on output requirement and investment budget Ingot type - ADC12 (7.5kg/ 10kg / customized) 1. After cleaning the oil and grease of waste aluminum, manually put it into the furnace with a forklift; 2. Ignition for melting furnace .Heat up to 680C, and input appropriate proportion of alloy elements. Heat up to 800C, melt and stir evenly, then fetch samples to the spectrometer for testing. Every lot of production need to do testing . 3. Put A tool that attracts iron into the furnace by forklift, to suck away the iron in the aluminum water. 4. Put the slag agent into Alu liquid to remove the slag. After slag removed , put the slags into Aluminum ash separation machine , and let the aluminum water and ash separate. The proportion of slag agent and aluminum liquid is 1:500 5.Open the drain valve and the aluminum water flows automatically to the ingot production line After the ingot casting is completed, the ingot stacking robot will stack the ingots, which means the production is completed.
Name of product : Cobalt Concentrate 10-20% and Cobalt Hydroxide 24-26% and grade 8-10%. Price of product : LME Cobalt x Co% x payable % on dry basis ex-warehouse Zambia. Exact payable % to be determined for quality required. Product origin : Zambia Key Specifications/Special Features Harmonization System (HS) Code : Minimum Order Size : 500 mt, but up to 2000 MT per month Packaging details : Big bags
We also have interest in selling Bulk Ferro Alloys and especially Low/Medium Carbon Silico Manganese and we are already exporting these product/s. We have tied up with a manufacturer bin , Bhutan to sell their products. Products are:- Low Carbon Silico Manganese. Typical Specifications are: Mn: 55 % Minimum Si: 25-28% C: 0.2% Maximum P: 0.15% Maximum Size: 10-150 MM (90%) Medium Carbon Silico Manganese. Typical Specifications are: - Mn: 55%-60% Si: 22%-25% Max C: 0.5% Max Si: 0.05% Max P: 0.2%-0.40% Size: 10-150 MM (90%) For sure, we will be able to meet the requirements, once we get your reply
Alloy 20 is an austenitic nickel-iron-chromium alloy with outstanding corrosion resistance. Alloy 20 Olets provide strong sulfuric acid resistance. This alloy is also resistant to phosphoric acid, nitric acid, and aqueous salt solutions. Alloy 20 Olets are an excellent choice when chloride stress corrosion cracking is a concern since they resist pitting and crevice corrosion. Because the rate of corrosion can substantially increase in chloride ion-containing environments, caution should be exercised. Alloy 20 Olets may provide cost savings while outperforming typical stainless steels when compared to higher nickel-based alloys. Alloy 20 is a super-austenitic stainless steel that was developed for maximum corrosion resistance to sulfuric acid and other extreme environments where regular austenitic grades are ineffective. Hot-working and cold-working are two traditional ways of producing Alloy 20. Itâ??s also vital to determine whether or not the desired corrosion resistance can be achieved in a given environment. Alloy 20 is used in a variety of industries, including chemical processing, petrochemical and refining, marine, pharmaceutical, and food processing. End-use applications include storage tanks, mixing tanks, agitators, pump and valve parts, food processing equipment, fasteners, and fittings. Plastics and synthetic fiber manufacturing Equipment for chemical and petroleum processing, heat exchangers, and process piping
Cobalt-chromium-molybdenum alloy (CoCrMo) is a kind of cobalt-based alloy, and is also a kind of Stellite alloy. It is a cobalt-based alloy that is resistant to wear and corrosion. The first cobalt-based alloy was a cobalt-chromium binary alloy, which was later developed into a cobalt-chromium-tungsten ternary composition, and then later did the cobalt-chromium-molybdenum alloy develop. Cobalt-chromium-molybdenum alloy is a kind of alloy with cobalt as the main component, containing a considerable amount of chromium, molybdenum and a small amount of nickel, carbon and other alloying elements, and occasionally also containing iron. DM FOR MORE IMFO
Price: -17%LME Origin: United States Delivery: FOB Payment terms:15% down payment through bank transfer followed by an irrevocable & confirmed documentary letter of credit payable against documents at the seller's bank.