Product introduction:
Dsc is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. Dsc research and development includes the following field: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (oit
Main features:
1. New designed oven structure ensures high resolution and good stability of base line;
2. Air flow meter may control the air flow rate accurately; the test data can be recorded into the database directly;
3. The instrument is bilateral control, may be controlled by both main frame and software. User-friendly interface, easy operation.

Technical parameters:
1. Dsc range: 0�500mw
2. Temperature range: -100 ~ 800 air-cooled
3. Heating rate: 1 ~ 80/min
4. Temperature resolution: 0.1
5. Temperature fluctuations:�0.1
6. Temperature repeatability:�0.1
7. Dsc noise: 0.01w
8. Dsc resolution: 0.01w
9. Dsc accuracy: 0.1w
10. Dsc sensitivity: 0.1w
11. Control mode: rising temperature, constant temperature(full automatic programmed control)
12. Curve scanning: rising scan, *cooling scan
13. Atmosphere control: embedded digital flow meter & software control
14. Color: 24 bit 7 inches lcd touch screen display
15. Data interface: standard usb connector
16. Parameter standard: equipped with standard material, with a key calibration function, the user may correct temperature and heat enthalpy
17. Note: * for selecting projects, all technical indicators can be adjusted according to customers' demand