High speed steel W6Mo5Cr4V2 Anneal temperature: 840-860oC Relief annealing temperature: 720-760oC Hardening temperature: 1210-1230oC Hardening medium: salt bath under 600oC,aslo use oil cooling or air cooling Normal temper temperation: 540-560oC RC Rockwell Hardness after hardening and temper: 63-66 Characteristic:Tungsten-molybdenum high speed steel developed by China, high performance in toughness, hardness, high temperature hardness. Application: Can be used in the manufacture of high capacity cutting tools to bear impact force ,such as gear shaper cutter, milling cutter,screw tap,drill bit etc.Also can be used in manufacture of large scale and thermoplasticity shaped cutting tools and antiabrasive cutting tools under high load.