Introduction: JERINA Plasticizer A is mixture of selected high molecular weight saturated fatty acid zinc salt. Technical Specification: Appearance: Yellow granule Melting point deg.: 100.0-104.0 Ash content (850degX2h),%: 12.0-14.0 Zinc content %: 12.0-14.0 Iodine value, g/100g: 40.0-50.0 Performance: 1. JERINA Plasticizer A can reduce the viscosity of natural and synthetic rubber to making it easy to process. 2. JERINA Plasticizer A can improve the dispersion of filler and rubber chemicals in the rubber compound, and improve scorch safety. It also can promote vulcanization and release of vulcanized products to keep the mold clean. 3. JERINA Plasticizer A canshorten the mixing time, change flowability of unvulcanized rubber, and there is no adverse effect on the bonding of rubber and metal material. It can improve storage stability of rubber compound, especially beneficial for vulcanization process. 4. JERINA Plasticizer A also can improve compression set performance when applied in sealing strip of EPDM. Application: 1. Add plasticizer A together with rubber compound. 2. Plasticizer A is applicable to NR, SBR, NBR, EPDM etc. 3. Suggested ratio: 1-5phr Packing and Storage: 1. It is packed in Kraft paper bags lined with plastic film, net weight is 25kg/bag. 2. It should be stored in a cool, dry warehouse. 3. The shelf life is 24 months.